Analysis of Alloy 718 surfaces milled by abrasive waterjet and post-processed by plain waterjet technology
Loading...
Identifiers
Publication date
2017
Authors
Advisors
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
This work analyzes the surfaces obtained in Alloy 718 when they are milled by Abrasive Waterjet (AWJ) at different conditions. This analysis revealed that all surfaces have a homogeneous roughness in the transversal and the longitudinal directions, present embedded abrasive particles and have hardened about 50% with respect to the untreated bulk Alloy 718. On the other hand, Plain Waterjet (PWJ) technology was used for removing the abrasive particles embedded in surfaces of Alloy 718 milled previously by AWJ technology. The effect of this process on the surface characteristics is also analyzed. For all tested conditions, this technology removed all the particles embedded in the surface. In addition, the PWJ technology process in general smoothened the surfaces produced by AWJ milling and it also released near-surface stresses.
Description
Publisher Copyright: © 2017
Keywords
Waterjet , Alloy 718 , Post-treatment , Milling , Fatigue , Waterjet , Alloy 718 , Post-treatment , Milling , Fatigue , Industrial and Manufacturing Engineering , Artificial Intelligence , Funding Info , The authors acknowledge the support of the Ministry of Economy and Competitiveness of the Spanish Government_x000D_ for support of project EVOCA II (reference DPI2013-45308-P). , The authors acknowledge the support of the Ministry of Economy and Competitiveness of the Spanish Government_x000D_ for support of project EVOCA II (reference DPI2013-45308-P).
Type
Citation
Alberdi , A , Rivero , A , Artaza , T & Lamikiz , A 2017 , ' Analysis of Alloy 718 surfaces milled by abrasive waterjet and post-processed by plain waterjet technology ' , Procedia Manufacturing , vol. 13 , pp. 679-686 . https://doi.org/10.1016/j.promfg.2017.09.163