Manufacturing and forging issues encountered while upscaling 1.3C30Mn10Al-austenitic and 0.65C12Mn-duplex low-density steels

dc.contributor.authorKaltzakorta, Idurre
dc.contributor.authorGutierrez, Teresa
dc.contributor.authorElvira, Roberto
dc.contributor.authorJimbert, Pello
dc.contributor.authorGuraya, Teresa
dc.contributor.institutionCIRMETAL
dc.date.issued2021-07
dc.descriptionPublisher Copyright: © 2021 Taylor & Francis.
dc.description.abstractDifficulties found when manufacturing and forging two low density steels in different scales are described in this work. Austenitic and duplex low-density steels have attracted a lot of interest due to their good combination of mechanical properties and density reduction. In this work, the fabrication of 1.3 C30Mn10Al austenitic low-density steel and 0.65 C12Mn10Al duplex low-density steel have been studied. The scaling up of the manufacturing process from 1 Kg to 35 Kg ingots of both materials and the subsequent hot forging of the ingots is described, showing the difficulties encountered during the production and transformation of these steels. Only the small ingots were successfully forged, but not the larger ones, showing the important differences in the forging properties depending on the geometry and dimensions of the final part to be forged, and the homogenization temperatures. The possible causes of this scale dependence are proposed from the experimental results obtained, as well as from the hot axial compression tests and the thermodynamic simulations carried out.en
dc.description.statusPeer reviewed
dc.format.extent12
dc.format.extent7473932
dc.identifier.citationKaltzakorta , I , Gutierrez , T , Elvira , R , Jimbert , P & Guraya , T 2021 , ' Manufacturing and forging issues encountered while upscaling 1.3C30Mn10Al-austenitic and 0.65C12Mn-duplex low-density steels ' , Materials and Manufacturing Processes , vol. 37 , no. 1 , pp. 43-54 . https://doi.org/10.1080/10426914.2021.1944192
dc.identifier.doi10.1080/10426914.2021.1944192
dc.identifier.issn1042-6914
dc.identifier.otherresearchoutputwizard: 11556/1163
dc.identifier.urlhttp://www.scopus.com/inward/record.url?scp=85109712209&partnerID=8YFLogxK
dc.language.isoeng
dc.relation.ispartofMaterials and Manufacturing Processes
dc.rightsinfo:eu-repo/semantics/restrictedAccess
dc.subject.keywordsLow-density steels
dc.subject.keywordsHot forging
dc.subject.keywordsFecmnal
dc.subject.keywordsGleeble
dc.subject.keywordsLow-density steels
dc.subject.keywordsHot forging
dc.subject.keywordsFecmnal
dc.subject.keywordsGleeble
dc.subject.keywordsGeneral Materials Science
dc.subject.keywordsMechanics of Materials
dc.subject.keywordsMechanical Engineering
dc.subject.keywordsIndustrial and Manufacturing Engineering
dc.subject.keywordsFunding Info
dc.subject.keywordsThis work was supported by the Basque Government under ELKARTEK Research Program[KK-2016/00029-ABADE] and [KK-2018/00016- COFADEN].
dc.subject.keywordsThis work was supported by the Basque Government under ELKARTEK Research Program[KK-2016/00029-ABADE] and [KK-2018/00016- COFADEN].
dc.titleManufacturing and forging issues encountered while upscaling 1.3C30Mn10Al-austenitic and 0.65C12Mn-duplex low-density steelsen
dc.typejournal article
Files
Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Manufacturing and forging.pdf
Size:
7.13 MB
Format:
Adobe Portable Document Format