dc.contributor.authorGómez, Iñigo
dc.contributor.authorGarcía, Jose Antonio
dc.contributor.authorSantiago, Jose Antonio
dc.contributor.authorFernandez, Iván
dc.contributor.authorJose Fernandez, Palacio
dc.contributor.authorBraceras, Iñigo
dc.date.accessioned2022-12-02T12:49:31Z
dc.date.available2022-12-02T12:49:31Z
dc.date.issued2022-11
dc.identifier.citationGómez, Iñigo, Jose Antonio García, Jose Antonio Santiago, Iván Fernandez, Palacio Jose Fernandez, and Iñigo Braceras. “Adhesion Enhancement on a Duplex DLC HiPIMS Positive Pulse Coating Performed by Active Screen Plasma Nitriding Pretreatment on 316L Stainless Steel Substrate.” Edited by Senthil Kumaran Selvaraj. Advances in Materials Science and Engineering 2022 (November 23, 2022): 1–11. https://doi.org/10.1155/2022/5621154.en
dc.identifier.issn1687-8434en
dc.identifier.urihttp://hdl.handle.net/11556/1444
dc.description.abstractDiamond-like carbon (DLC) coatings have been the object of research interest due to properties such as excellent wear resistance, low coefficient of friction, high hardness, high elastic modulus, and biocompatibility. Despite this, DLC has poor adhesion properties, which makes it challenging to use in industrial applications. The application of DLC using the high-power pulse magnetron sputtering (HiPIMS) technique with positive pulses has been studied. Seeking greater DLC coating adherence, the application of a nitriding pretreatment prior to the DLC coating has been studied to improve its adhesion to AISI316L stainless steel soft metal substrates, employing active screen plasma nitriding (ASPN). The influence of the different pretreatment temperatures to reach the maximum levels of adhesion has been analyzed. Scratch methods have been employed to assess adhesion. The elemental composition, morphology, and roughness of the samples have been studied, as well as the behavior of resistance to wear and friction. The results show an improvement in DCL adhesion. Critical loads (LC3) increase at higher pretreatment temperatures, from 48 N for the DLC to 82 N for the ASPN + DLC. Pretreatment has also been shown to be effective in maintaining excellent dry wear resistance properties and a low coefficient of friction.en
dc.description.sponsorshipThis research was supported by the Government of Navarra grants for hiring doctoral students (Iñigo G´omez) by companies and research and knowledge dissemination organizations: industrial doctorates 2019–2021, grant no. 0011-1408-2018-000000 and CDTI Ministerio de Ciencia e Innovaci´on of Spain through the project CERVERA (CER2019-1003).en
dc.language.isoengen
dc.publisherHindawien
dc.rightsAttribution 4.0 International*
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/*
dc.titleAdhesion Enhancement on a Duplex DLC HiPIMS Positive Pulse Coating Performed by Active Screen Plasma Nitriding Pretreatment on 316L Stainless Steel Substrateen
dc.typearticleen
dc.identifier.doi10.1155/2022/5621154en
dc.rights.accessRightsopenAccessen
dc.subject.keywordsDiamond-like carbon (DLC) coatingsen
dc.subject.keywordsAdhesion propertiesen
dc.identifier.essn1687-8442en
dc.journal.titleAdvances in Materials Science and Engineeringen
dc.page.final11en
dc.page.initial1en
dc.volume.number2022en